Ultraclean coals represent an important raw material to elaborate high value products such as carbon fiber, electrodes, carbon foam and so on. In this work, ultraclean coals having less than 0.50% (w/w, db) of ash and 1.00% q(w/w) of mineral matter were obtained using flotation column and leaching with acid fluorhídric (HF) and nítric (HNO3 ). Ash content was reduced from 19.60 to 8.70 %, using three flotation stages. Chemical processing, using HF 7.53 M and HNO3 2.30 M, produced 1.42% of ash content, 0.86 % of sulphur and 2.00% of mineral matter, whereas a combined process, froth flotation followed by leaching of HF 19.2M and HNO3 8.12M produced a coal having 0.48 % of ash content, 0.71% of sulphur content and 0.96% of mineral matter. However, when it was used the original coal (unfloated) at the same acid conditions of the combined process, it was obtained an ultraclean coal having 0.33% of ash content.
Tópico:
Minerals Flotation and Separation Techniques
Citaciones:
0
Citaciones por año:
No hay datos de citaciones disponibles
Altmétricas:
0
Información de la Fuente:
FuenteRevista Facultad de Ingeniería Universidad de Antioquia